ASME B31.3 Para 328.2.2 Interpretation

242 views
Skip to first unread message

Babur Khan

unread,
Mar 3, 2021, 1:19:17 AM3/3/21
to material...@googlegroups.com
Dear Experts,
Please clarify ASME B31.3 para 328.2.2 Procesure Qualification by Others 
My question is 
Can the Sub Contractor utilized Main / EPC Contractor  WPS for same project?
As per Interpretation number B31.3-18-07
Question (1): In accordance with ASME B31.3-2016, may a contractor follow a WPS that has been qualified by another company in accordance with the requirements of para. 328.2.2?
Reply(1): Yes
Question (2): In accordance with ASME B31.3-2016, does para 328.2.2 take precedence over the rules of ASME Section IX?
Reply (2): Yes
Please share your knowledge and experience for above questions.

Muhammad Babur Khan
Cell # 00966 582774568
Sent from my iPhone

Raghuram Bathula

unread,
Mar 3, 2021, 1:20:35 AM3/3/21
to Materials-Welding
Yes

--

james gerald

unread,
Mar 3, 2021, 1:47:49 AM3/3/21
to material...@googlegroups.com
Yes you can use it subject to the Approval of Client / Owner.

Thanks & Regards

J.Gerald Jayakumar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/69A4617A-28EA-404D-AEB0-FA09817C87CA%40gmail.com.

james gerald

unread,
Mar 3, 2021, 2:47:27 AM3/3/21
to 'james gerald' via Materials & Welding
Just to add, without invoking the below clause still you can use it provided the subcontractor is included in your Quality procedure as under the Operational control of Main/EPC contractor.

Thanks & Regards

J.Gerald Jayakumar