WPS QUALIFICATION WITH CLADDING.

181 views
Skip to first unread message

hemant

unread,
Jan 24, 2013, 8:22:21 AM1/24/13
to material...@googlegroups.com, Hardik Pandya, pravi...@yahoo.co.in

Dear Sir,

We going to tube to tube sheet joint with as below given material, our tube to joint is groove fillet weld as shown in sketch. I have to qualify WPS for SB 575 to 316L. we have only  SB 575 50mm thick tube sheet material. And 316L plate.

Can I qualify WPS with fillet weld?  Or can I used 316L plate with ERNiCrMo4 cladding and 316L plate for plate to plate qualification.

 

Pls reply.

 

TUBE SHEET- ASTM SB 575, UNS N10276

SHELL-SA 312 TP 316L

 

 

HEMANT SUTHAR

QA/QC

CEPL-SILVASSA

9712973092

 

image001.png

Prakash Hegde

unread,
Jan 25, 2013, 3:16:37 AM1/25/13
to material...@googlegroups.com, Hardik Pandya, pravi...@yahoo.co.in
D

-
Dear Hemant 
In your case It is of Tube sheet to shell joint (as per your sketch) Please refer QW 202.4 of ASME sec IX which is self explainatory  and you can qualify PQR accordingly ( In your case it is P43 to P8
Regards
Hegde P.B.

Regards
From: hemant <hsu...@chemithon.co.in>
Subject: [MW:16585] WPS QUALIFICATION WITH CLADDING.
To: material...@googlegroups.com
Cc: "Hardik Pandya" <hardi...@yahoo.co.in>, pravi...@yahoo.co.in
Date: Thursday, 24 January, 2013, 6:52 PM

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 