I would like to know what is the permissible limit of offset between 2 longitudinal seam especially for piping. ASME VIII clearly stated but B31.3 silent on it. Any other reference, code or recommended practice that i can refer to it. If any could you share with me. Thank in advance for you cooperation
Regards
Su

Pablo Acelajado

unread,
May 14, 2009, 1:32:22 AM5/14/09
to material...@googlegroups.com

May 14, 2009

 

Su,

 

For line pipes, API 5L/ISO 3183, edition 2007, radial offset or misalignment allowed for SAW depends on wall thickness (WT):  lesser than or equal to 15.0 mm WT allowed is 1.5mm; greater than 15.0 mm to lesser than or equal to 25.4 mm WT allowed is 0.10 of WT; and greater than 25.4 mm WT allowed is 2.5 mm.

Best regards.

 

PJA

SAVE TREES  - THINK BEFORE YOU PRINT


Reply all
Reply to author
Forward
0 new messages