            Kindly share your experiences (special precautions to be taken) during Strength Welding of 


            Aluminium Brass Tube -‘SB 111 UNS C68700’ (78Cu-20Zn-2Alto  

            Aluminium Bronze Tube sheet -‘SB 171 UNS C61400’ (90Cu-7Al-3Fe).

           