inconel welding electrode

85 views
Skip to first unread message

Ilangkumaran Kumarasamy

unread,
Feb 1, 2011, 6:46:05 AM2/1/11
to material...@googlegroups.com

Dear experts,

 

                        I have used sec II part C, for selecting electrodes and filler wires with sec IX, F no etc,. There is separate para for nickel and nickel alloys in sec IX. Eg F no:43  Now what is this Inconel welding electrode 82/ 182? Is there any different name for some other materials?

 

Can somebody explain me?

 

Ilan

 

 

**********************************************************************

Borouge is a leading provider of value creating, innovative plastics solutions for customers in the Middle East, Asia-Pacific and Africa. Borouge employs unique Borstar® technology to produce differentiated products for high-value infrastructure applications, including water, gas and industrial pipe systems, power and communication cables, advanced packaging and automotive components. Borouge’s state-of-the-art petrochemical complex is located at Ruwais, Abu Dhabi in the United Arab Emirates.

===================================================================================
CONFIDENTIALITY NOTICE

This email and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this email in error please delete the email and any attachment(s) and notify the sender.

This footnote also confirms that this email message has been scanned for the presence of computer viruses.
=============================================================================================================

 

John Henning

unread,
Feb 1, 2011, 12:17:58 PM2/1/11
to material...@googlegroups.com

International Nickel Company (INCO) was the originator of welding electrodes with compositions now designated as ASME Section II, Part  C, SFA-5.11 ENiCrFe-3 {SMAW) and SFA-5.14 ENiCr-3 {GTAW/GMAW}.    The registered trademarked names for these are INCONEL Welding Electrode 182 and INCONEL Filler Metal 82 respectively.  Recognition of INCO’s development, trade mark, and, ultimately, common usage, can be seen in the assigned UNS numbers;  i.e.  W86182  and N06082.  F43 encompasses a number for filler metal compositions including  ENiCrFe-3 and ERNiCr-3 as you can see by reviewing ASME Sc IX, QW-432.

 

John

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Ilangkumaran Kumarasamy
Sent: Tuesday, February 01, 2011 5:46 AM
To: material...@googlegroups.com
Subject: [MW:9650] inconel welding electrode

 

Dear experts,

 

                        I have used sec II part C, for selecting electrodes and filler wires with sec IX, F no etc,. There is separate para for nickel and nickel alloys in sec IX. Eg F no:43  Now what is this Inconel welding electrode 82/ 182? Is there any different name for some other materials?

 

Can somebody explain me?

 

Ilan

 

 

**********************************************************************

Borouge is a leading provider of value creating, innovative plastics solutions for customers in the Middle East, Asia-Pacific and Africa. Borouge employs unique Borstar technology to produce differentiated products for high-value infrastructure applications, including water, gas and industrial pipe systems, power and communication cables, advanced packaging and automotive components. Borouges state-of-the-art petrochemical complex is located at Ruwais, Abu Dhabi in the United Arab Emirates.

===================================================================================
CONFIDENTIALITY NOTICE

This email and any files transmitted with it are confidential and intended solely for the use of the individual or entity to whom they are addressed. If you have received this email in error please delete the email and any attachment(s) and notify the sender.

This footnote also confirms that this email message has been scanned for the presence of computer viruses.
=============================================================================================================

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.