Low alloy vs high alloy steel

55 views
Skip to first unread message

mithlesh kumar

unread,
Dec 28, 2022, 1:23:52 AM12/28/22
to Materials & Welding
Dear expert ,

Please brief difference between low alloy steel vs high alloy steel.

A335 P9 is low or high alloy steel.

Sankaran Sp

unread,
Dec 28, 2022, 10:31:36 PM12/28/22
to Materials & Welding
Dear Mr. Mithlesh kumar,

when we adding the total alloying elements of Cr,Ni,Mo, if the total is less than or equal to 10% this is low alloy steel, total alloys are greater than 10 % that is high alloy steel.

A335 P9 - low alloy steel pipe.     

Regards,
Sankaran.SP
Welding & Metallurgy expert
Coimbatore, India. 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/62edc733-0051-4b57-9c08-171a8ff85d71n%40googlegroups.com.

Kannayeram Gnanapandithan

unread,
Dec 29, 2022, 10:18:03 PM12/29/22
to material...@googlegroups.com
Low alloy less than 5% of individual or aggregate of total number of alloying elements ,  greater  than 5% and less than 10.5% is medium, and above 10.5 high alloy as mentioned for low alloy.
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,