Dear Gents

If we have WPS with two materials, P-1 to P-8 and impact test required,
According to ASME B31.3, we can apply impact test on one side only ( carbon steel) ?
Or shall be applying impact test on SS with CS ?

Please advise 


Thanks,

Hany Nabil
Welding Engineer 
--


 Best Regards,

 Eng. Hany Nabil
 Senior QA / QC Welding Engineer
 Egypt Mobile: 002-01225622022


This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorised to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.

George Dilintas

unread,
Dec 16, 2021, 11:10:13 PM12/16/21
to material...@googlegroups.com
Impact test is applicable for weld metal and both heat affected zones. You follow B31.3 to the letter

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP1YJmRrDRHB-c2Y_cmmyN8A0B%3DMGqJ59g-SKdAtmc6ObptjAw%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Hany Nabil

unread,
Dec 17, 2021, 2:23:46 AM12/17/21
to material...@googlegroups.com
Dear Mr. George

Thanks 
But I think impact test required on minimum tensile strength only.

Can you explain me which reference article in ASME B31.3

Thanks 
Hany Nabil

james gerald

unread,
Dec 19, 2021, 6:16:58 AM12/19/21
to material...@googlegroups.com
According to ASME B 31.3, Impact requirements based on Table 323.2.2 and for P1 & P8 materials as specified in that section. Consider the base metal weld & HAZ requirement and exception according to the above table.

If weld requires impact test then the below acceptance criteria apply.

Inline image
Inline image


Table 323.2.2 as below.


Inline image

Thanks & Regards

J.Gerald Jayakumar