Welder Qualification Combination

46 views
Skip to first unread message

Babur Khan

unread,
Jan 21, 2017, 3:03:31 AM1/21/17
to material...@googlegroups.com
Dear Experts,

We have a confusion detail below.

We have Qualified Welders for different WPS, Process, Diameter and thickness range.

1)  Welder Qualified on CS OD 2" and Thickness 5.54(11.08) GTAW Process.
2) Same Above welder qualified above OD 2" and Thickness 12.7(25.4)      GTAW+SMAW Process.

Now We have 2" Pipe Thickness 11mm and 15mm and WPS Detail below
GTAW 9mm qualification.
GTAW+SMAW 25.4mm.

We can use above welder for 2" pipe with 15mm Thickness?

Regards,

Muhammad Babur Khan Lashari
Sr. QA/QC Inspector

(CSWIP 3.1 / CWI II From PWI) 

 Khaled Juffli Industial Company

Mob: + 966 56 2179280 / 58 2774568

PAK : + 92 334 6186285

Skype: babur.lashari

E-Mail: babur...@kjgroup.com

George Dilintas

unread,
Jan 24, 2017, 9:57:16 PM1/24/17
to Meghanadh K
When a welder is qualified for two processes with a single coupon, the deposited weld metal thickness has to be recorded separately for each process

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN53wK3Tc95cp-Tma_r2SByxayUo4pqAaPmyQf-t_P%3DvztmAnQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Manoj Singh

unread,
Jan 24, 2017, 9:58:00 PM1/24/17
to material...@googlegroups.com

No ,if your spec says  full gtaw for 2" and below size

--
Reply all
Reply to author
Forward