IMPACT TESTING FOR ASTM A193 L7 MATERIAL STUD
54 views
Skip to first unread message
Mahesh Purohit
unread,
Apr 3, 2023, 3:48:52 AM
4/3/23
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding
Dear Sir
We have an requirement for ASTM A193 GR.L7 stud with impact testing @ -120deg C
Kindly suggest your best opinion
james gerald
unread,
Apr 3, 2023, 5:45:10 AM
4/3/23
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to material...@googlegroups.com
There is no specification as such as ASTM A 193 Gr. L7, Only ASTM A320 L7 exists with Impact test requirement at -101degC
Thanks & Regards
J.Gerald Jayakumar
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com
.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/ec09c075-4414-4d47-ae2f-b2187ddb7f02n%40googlegroups.com
.
Reply all
Reply to author
Forward
0 new messages