IMPACT TESTING FOR ASTM A193 L7 MATERIAL STUD

55 views
Skip to first unread message

Mahesh Purohit

unread,
Apr 3, 2023, 3:48:52 AM4/3/23
to Materials & Welding
Dear Sir 

We have an requirement for ASTM A193 GR.L7 stud with impact testing @ -120deg C 

Kindly suggest your best opinion 

james gerald

unread,
Apr 3, 2023, 5:45:10 AM4/3/23
to material...@googlegroups.com
There is no specification as such as ASTM A 193 Gr. L7, Only ASTM A320 L7 exists with Impact test requirement at -101degC

Thanks & Regards

J.Gerald Jayakumar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ec09c075-4414-4d47-ae2f-b2187ddb7f02n%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages