Difference between ASTM and API pipes

382 views
Skip to first unread message

N VENKATESWARA PRASAD

unread,
Jun 9, 2010, 9:25:57 AM6/9/10
to material...@googlegroups.com
Hi,
 
Any body can tell what is major differences between ASTM and API pipes.  Whay we can not use A 106 Gr.B in  place of API 5L Gr. B.  Why ASTM spec. pipes are not used for pipe lines.  Is there any supply conditions are diffrerent or test required are different.
 
please share your ideas.
 
Regards
 
N.V. PRASAD
Welding engineer, Velosi

Suresh

unread,
Jun 9, 2010, 12:48:14 PM6/9/10
to material...@googlegroups.com
Prasad,
 
It is all depends on design criteria and strength.API 1104 code is specially made for pipelines .If you see deeply ,there is not much difference between them .Ex: chemical & mechanical properties are bit same.
 
Regards
 
Suresh
 
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh