k c

unread,
Aug 26, 2016, 12:37:08 AM8/26/16
to material...@googlegroups.com
Dear All

Can any body suggest code required testing, for the welding done after hydro test.

this welding is done on hydro tested shell,  after hydro test. Code vessels and U Stamping required.

Best Regards
K C R

pgoswami

unread,
Aug 26, 2016, 11:55:33 PM8/26/16
to material...@googlegroups.com

Hi KCR,

 

You need to repeat the hydro test following. Please see Sec-VIII, DIV-1, UG 99 (a) (1). Also see the following discussion in Eng Tips discussion forum also:- http://www.eng-tips.com/viewthread.cfm?qid=212412.

Depending on the design codes there could be some relaxations.

 

However the default rule, is to repeat the hydro test after any further welding.

 

Thanks.

 

 

Pradip Goswami, P.Eng,IWE

Welding & Metallurgical Engineering Specialist ,
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgos...@quickclic.net

pradip....@gmail.com

H-905-6799677, 905-9631505

C-905-9793232

 


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL9TLdcUnFv1zzSgYJ82nqzg7L72P3QdihuNtYKLMSJjaOZDXA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Reply all
Reply to author
Forward
0 new messages