Dear All.

In ASME IX, don't use ''shall'' for longitudinal bend test for dissimilar joint, now if contractor used side bend test for it's PQR and after retesting satisfactory result reached, we can accept it or not?

In ASME IX, criteria for bending of clad is 1.5mm but can extended to 3 mm if occurred in interface, now if we observed a defect with length less than 3 mm that some of length of it is in fusion line of clad and base metal, is it accepted or not?

Regards

Kannayeram Gnanapandithan

unread,
Mar 6, 2019, 10:43:49 PM3/6/19
to materials-welding
Where it is mentioned for Longitudinal bend test for dissimilar material

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Ali Asghari

unread,
Mar 7, 2019, 11:30:09 AM3/7/19
to material...@googlegroups.com
Dear Mr.
QW-161.5
Regards.

You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/U8dnftQ8w4o/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.

HENNING John

unread,
Mar 7, 2019, 11:30:09 AM3/7/19
to material...@googlegroups.com

The longitudinal bend test is an optional alternate to the cross weld bend test for dissimilar metal welds.  When there are significant differences in material properties that will result in fracture of the side bend tests you can opt to do a longitudinal bend test.  It is not a requirement but an option. 


______________________________________________________________________
DISCLAIMER This e-mail and any attachments thereto may contain information which is confidential and/or protected by intellectual property rights and are intended for the sole use of the recipient(s)named above. Any use of the information contained herein (including, but not limited to, total or partial reproduction, communication or distribution in any form) by persons other than the designated recipient(s) is prohibited. If you have received this e-mail in error, please notify the sender either by telephone or by e-mail and delete the material from any computer.
General Data Protection Regulation (GDPR)
We respect and protect your privacy to provide you with our services. Please read https://www.hamon.com/customer-data-protection-notice (Customer) and https://www.hamon.com/seller-data-protection-notice (Supplier) how we process your personal data.

Thank you for your cooperation.
______________________________________________________________________
Reply all
Reply to author
Forward
0 new messages