Incoloy 800H / N08810

26 views
Skip to first unread message

King Captain

unread,
Aug 29, 2025, 12:09:07 AMAug 29
to Materials & Welding
Dear expert.

I have this question. My client is looking for Incoloy 800H, which must be NACE MR0175 Part 3 compliant. he wants our issue MTC with NACE.

Isn't incoloy 800H just satisfied with NACE. I only saw Carbon steel marked with NACE, but never seen NACE mark on SS.

Can anyone with knowledge explain this

Best

Harish Kannepalli

unread,
Aug 29, 2025, 12:27:03 PMAug 29
to material...@googlegroups.com
Hi,
    NACE MR0175-3 describes requirements of corrosion resistant alloys, which covers Inconel alloys. 

Regards,
Mr. Harish.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/d21594a7-f3e6-4fbc-9408-fc420aedd166n%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages