testing of inaccessible welded joints

37 views
Skip to first unread message

Ali Asghari

unread,
Sep 23, 2018, 3:52:52 AM9/23/18
to Materials & Welding
Dear All.

Does anybody know there is NDT method that can inspected welded joints which are buried and not accessible?our concern is about finding of construction defects either surface and internal that have a good detect ability for linear ones particularly Transverse Crack.

Regards.
 

Lakshmankumar Bayyana

unread,
Sep 23, 2018, 6:02:00 AM9/23/18
to material...@googlegroups.com
If it is a pipe line, best option is to do hydro test with 1.25 times of the working pressure to ensure the integrity 
Also can go with ultrasonic pig in case of pig possible lines

Thanks and Regards 
Lakshman kumar. B 

Sent from my iPhone
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Ali Asghari

unread,
Sep 23, 2018, 8:17:28 AM9/23/18
to material...@googlegroups.com
Dear Kumar.
this line is piggable but I don't think the pig with considering pf it's velocity don't have ability to scan welds?if you know information or experience, please let me know.
pressure testing can only detect defects that cause leak or rupture, and other rejected defects can be undetected.

Regards.

You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/U-K3LErE3mU/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.

sandeep kumar

unread,
Sep 24, 2018, 1:07:18 AM9/24/18
to Materials & Welding
for smaller length, a surface inspection with boroscope can be possibly made. Now a days boroscope with robot manipulator (pipe crawler) also available which can be remotely controlled although a costly matter.

The above system can be used upto 500 mm however diameter restriction is applicable.


Shared more details about the joint types, pipe dia length etc would be better for the understanding.

Thanks & regards
Sandeep Kumar

Ali Asghari

unread,
Sep 24, 2018, 3:31:44 AM9/24/18
to material...@googlegroups.com
Thank you for responding but our line is long& we want to know about internal defects and visual in that situation doesn't have good sensitivity.
Actually, I am wondering about mechanised ultrasonic that syncronised with crawler.
If you know any equipment or company that have simillar technology.
Regards.

pradip kumar Sil

unread,
Sep 26, 2018, 10:15:09 PM9/26/18
to materials-welding
Borodcope you can identify internal defect. otherwise pressure test

Ali Asghari

unread,
Sep 27, 2018, 3:00:26 AM9/27/18
to material...@googlegroups.com
Do you have any file for presenting this method?
I said in previous emails, pressure testing may not detect some rejected defects that don,t cause leak.
Regards.

Shashank Vagal

unread,
Sep 27, 2018, 3:45:46 AM9/27/18
to material...@googlegroups.com
Try Crawler RT

Best Regards,

Shashank C Vagal (Quality Adviser), (+91) 8082395502, 8779046302,

NEO METAL-ANALYST & NDT SERVICES

·       A-25, Geet Siddhi, Boradevadi, Moshi-Haveli, PCMC, Pune 412105

·      301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA

www.neometalanalystndt.com / enq...@neometalanalystndt.com / nach...@yahoo.com




Ali Asghari

unread,
Sep 27, 2018, 6:04:52 AM9/27/18
to material...@googlegroups.com
It is not possible since all of joints butied.
Does anybody know about high resolution MFL would be useful in evaluting of joint
Regards.
Reply all