Dear All,
How we can identify the number of wires(Range of wire like ISO penetrameter numbers 1-7,6-12,10-16) in DIN penetrameter?I have a RT film with DIN 62 FE penetrameter.What is the wire range of this penetrameter(To get the diameter of essential wire to calculate the sensitivity)?I have reference of all other penetrameters like EN,ISO and ASTM.Unfortunately,I am clueless about DIN.
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
|
3.20 |
2,50 |
2,00 |
1,60 |
1,25 |
1,00 |
0,80 | ||||||||||
|
6-12 |
1,00 |
0,80 |
0,63 |
0,50 |
0,40 |
0,32 |
0,25 | ||||||||||
|
10-16 |
0,40 |
0,32 |
0,25 |
0,20 |
0,16 |
0,125 |
0,10 | ||||||||||
| IS THERE ANYTHING LIKE DIN 62 FE penetrameter? --- On Sat, 30/10/10, Kale, Bhaskar M <bmk...@gmail.com> wrote: |