Redo the Hydrotest after the PWHT and NDT.

Regards,

On Fri, Jul 18, 2025 at 2:11 AM <material...@googlegroups.com> wrote:
Kannayeram Gnanapandithan <kgpan...@gmail.com>: Jul 17 02:05PM +0530

*Dears*
* Materials P11,P91 & LTCS.*
* Is there any provision to perform PWHT after Hydrotest without having to
repeat the Hydrotest again ?*
 
*THANKS & BEST REGARDS,*
*KG.PANDITHAN, BE, ...more
sridhar cn <sridha...@gmail.com>: Jul 17 07:46PM +0530

*For main pressure welds on materials like P11, P91, and LTCS, **PWHT is
essential when prescribed, and the integrity test (hydro) *
*must **follow all heat treatments unless the code or a ...more
You received this digest because you're subscribed to updates for this group. You can change your settings on the group membership page.
To unsubscribe from this group and stop receiving emails from it send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages