 Dear experts

whats the L.O.P Visual Inspection Acceptance Criteria according to AWS D1.1 ?

Best regards

Pieper QSI

unread,
Oct 3, 2015, 8:26:28 AM10/3/15
to material...@googlegroups.com

Dear Sir

 

Regarding table 6.1 point 2 – weld/base metal fusion complete fusion is required so lack of penetration is not allowed for full penetration welds. For partial penetration welds the actual depth of penetration can’t be examined by visual examination.

 

Met vriendelijke groeten / Best Regards,

 

Herman Pieper

QA-QC Inspector / CSWIP + IWI-C Welding Inspector / IWT / Materials Expert

 

Logo nieuw klein

Job van der Havestraat 6

8384 DB, Wilhelminaoord

Cell: +31 6 51691215

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/60468822-24e4-4a64-8127-db4fde3a250a%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

image001.jpg

Tarek Yehia

unread,
Oct 4, 2015, 11:54:50 AM10/4/15
to material...@googlegroups.com
Dear Mehdi,

Referring to AWS D1.1 Table 6.1 "Complete  fusion shall exist between adjacent layers of weld metal and between weld metal and base metal" but if the joint welding symbol mentioned CJP, BG, FP then no acceptance criteria for LOP.



-- 
Best regards,
 
Tarek Yehia