DINESH KUMAR DEVENDHIRAN

unread,
Sep 1, 2021, 7:50:09 AM9/1/21
to Materials & Welding
Dear Experts
I need a clarification on AWS table 4.1 vs 4.10
As per table 4.1- for 3G position WPS shall be qualify for vertical position only
As per table 4.10 - for 3G position welder will qualify for Flat, Horizontal, vertical.

My doubt is if i have a WPS for 3G uphill position, can i use the same WPS for 1G&2G also ?
If not please explain.

harenath jha

unread,
Sep 1, 2021, 11:26:46 AM9/1/21
to material...@googlegroups.com
Yes you can use it

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/571704be-652c-417c-9c67-6400ec82034an%40googlegroups.com.

Manikandan J

unread,
Sep 1, 2021, 11:27:26 PM9/1/21
to material...@googlegroups.com
Hai,

If your welder tested in 3G Position he can weld F,H & V Position.

3G PQR Will support only Vertical Welding.

If you need F&H position you need to establish New pqr with 2G position.

Regards,
Manikandan
9791367960

On Wed, Sep 1, 2021, 9:03 PM Manikandan J <mechm...@gmail.com> wrote:
Hai,

If your welder tested in 3G Position he can weld F,H & V Position.

3G PQR Will support only Vertical Welding.

If you need F&H position you need to establish New pqr with 2G position.

Regards,
Manikandan
9791367960






Vishwas Keskar

unread,
Sep 1, 2021, 11:37:07 PM9/1/21
to material...@googlegroups.com
AWS Table  is very clear for WPS PQR.
For each position ,PQR is needed .

Qualify PQR positions based on  envising Production Welding Joint positions.

For Welder , range for Qualified position is given based on WPQ tested position.




--

james gerald

unread,
Sep 5, 2021, 5:17:20 AM9/5/21
to material...@googlegroups.com
Older version of code referred in the query.

These are 2 different entities. 

 Table 4.1 is applicable only for WPS / PQR Qualification and hence you cannot use a WPS qualified in 3G position for 2G position WPS and you need to qualify a WPS for 2G position (according to Table 4.1 2G WPS qualifies for 1G position WPS also).

Table 4.10 is exclusively for Welder Qualification.

Inline image
There is an ambiguity in section 4.19.1 which refer to Table 4.11 as below.
Inline image
Inline image

In the Latest AWS D1.1 2020 edition it has been corrected.

Inline image


Hence the Welder who welded WPS for 3G position is also Qualified to weld 2G & 1G position.




Thanks & Regards

J.Gerald Jayakumar



--

Xuân Thông

unread,
Sep 5, 2021, 5:17:49 AM9/5/21
to material...@googlegroups.com
Dear sir, 
Please note that qualification for WPS and welder are deference
For welder, he can weld F, H, V but PQR/ WPS must be qulified more 
Vào Th 5, 2 thg 9, 2021 lúc 10:37 Vishwas Keskar <vvkes...@gmail.com> đã viết:

Mhaskar Aly

unread,
Dec 9, 2021, 10:21:20 PM12/9/21
to material...@googlegroups.com
With 3G WPS, you can qualify welder in 3G position which gives qualifications of flat, Horizontal and Vertical position to welder.

But for welding in Vertical, Horizontal and flat position you need WPS qualified in 2G and 3G position as per AWS D1.1.

But in AWS D1.6; qualification in one position gives qualification range as all positions.


Mhaskar Ali 
Dubai 

Chandan Singh

unread,
Dec 12, 2021, 2:50:15 AM12/12/21
to material...@googlegroups.com
Hi,

Position is non essential, that's why not required addition WPS & PQR.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/571704be-652c-417c-9c67-6400ec82034an%40googlegroups.com.


--
Regards
CHANDAN SINGH
Sterling & Wilson 
+919981575817
+917379619175


Mhaskar Aly

unread,
Dec 13, 2021, 10:20:26 PM12/13/21
to material...@googlegroups.com
Don't write anything, it will confuse others.
It's not Asme sec IX we are talking about.

Refer AWS D1.1...position is essential variable...PQR in 3G position qualifying vertical position only.
2G qualify flat and horizontal 



Sandeep Raghavan

unread,
Dec 14, 2021, 12:37:32 AM12/14/21
to material...@googlegroups.com

Dear Dinesh,

 

Please Keep in Mind that Procedure Qualification & Welder Qualification have different Criterions for Range of Qualified Welding Position.

 

For Procedure Qualification, Clause 6.4(AWS D1.1 Ed:2020) explains about the Range of qualified Welding Position.(Directing to Table 6.1 for Plates & Table 10.8 for Tubular Products). You can refer Table 6.5 for PQR Essential variable changes Requiring Requalification.

 

For Performance Qualification, Clause 6.16.1(AWS D1.1 Ed:2020) explains about the Range of qualified Welding Position .(Directing to Table 6.10 for Plates & Table 10.12 for Tubular Products). You can refer Table 6.12 for Welding Personnel Performance Essential variable changes Requiring Requalification.


With regards,

Sandeep.Raghavan

Shahil Saini

unread,
Dec 14, 2021, 6:09:36 AM12/14/21
to material...@googlegroups.com
Hello Manikandan Sir

Sir, can you tell me where I can find that welder is qualified for which position? and if the welder is qualified in any one of the positions, then in which other position welder is eligible for welding using one qualified position.
In which code can I find this position's qualifications of the welder?

Thank you sir


james gerald

unread,
Dec 14, 2021, 6:45:40 AM12/14/21
to material...@googlegroups.com
Dear,

I suppose your Applicable code is AWS D1.1

Please refer Table for PQR/WPS Qualification.

Inline image
For Welder Qualification refer below table.

Inline image


Thanks & Regards

J.Gerald Jayakumar


Reply all
Reply to author