Impact test possible at -269 degree celcius for Helium line

31 views
Skip to first unread message

MEENAKSHI SUNDARAM

unread,
Oct 26, 2016, 7:03:14 AM10/26/16
to Materials & Welding
Dear All,
Could you please advice that,Design temperature for Helium line -269 Degree Celsius. So I have to conduct PQR on design temperature but I have verified in Gulf countries,USA and Singapore Lab which is not possible to carry out at this temperature due to safety concern.

Anybody have done the impact at -269 degree Celsius. please provide the reference Lab to contact.

Material ASTM A312 TP 304L and 316L

Design code ASME B31.3,

Any alternative provision is available as per Design code like ASME B31.3,ASME Sec-VIII DIV -1 & 2 ,British code etc.

anthony chundal

unread,
Oct 26, 2016, 9:39:03 AM10/26/16
to material...@googlegroups.com
Dear,

It is done in Europe,I guess in Italy, they do  it in Helium, other places it is done in liquid nitrogen which will give only -196 deg celsius.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9647811f-55dc-4b82-9a17-cc2d036f4164%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Reply all
Reply to author
Forward
0 new messages