Dear all,
I want to weld 2inch weldolet to 24inch pipe, my doubt can i use welder qualified as per section 9 with diameter range 73mm and above to weld 2 inch weldolet whose OD is above 73mm.
Second doubt how much weld i need to deposit on weldolet to run pipe connection if code of construction is asme B31.3, i think it should be minimum thickness of branch or run pipe thickness and then make fillet. Or is it needed to deposit weld upto bevel end then a fillet.
Regards
Vikas
Dear vikas,
You have to qualify welder in 2 inch to weld that weldolet on 24 inch pipe....
Regards,
Vivek
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BCgecnc-uScigVNxcd15GJQmb8ZhT-SWKO2eoFX%2BJhg7%2Bkpyw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Dear all,
Thickness of both base materials also shall be considered as per Qw202.
Regards,
Anthony.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFOZxBj6SVzj%2B7RFXREdsRGSqgM_5Xm2MvR8Dr3Z9O-sD0gr2w%40mail.gmail.com.
Dear Friend,
2" Weldolet od will be more than 73mm and section 9 talks about OD.
My interpretation says we can weld , is there any code case or interpretation file number regarding same, if any of you arr aware please share.
Regards
Vikas
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOi%3DZp-Y8OUuuuHgt4-LD4%3DYfEe8TQcLUBVjqOnXbsAB8s3apA%40mail.gmail.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BCgeck7VQfFCXvCdgg2%3D5QPZKb0voqs862boMCr%3DWqVQeUunQ%40mail.gmail.com.
Dear Sir,
The welder diameter qualification range is 73mm and above, as he welded 6inch pipe.
My question is can the above said welder can do welding on 2inch weldolet to run pipe connection, as the weldolet od if physically verified will be more then 73mm.
Regards
Vikas
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40A8urMWfvbbo5iE9iR0BmfZDHSCYNfMtMtzZXO_xuWtyA%40mail.gmail.com.
Dear All,
One question
ASME JOB - ASME U STAMP certified company name ABC -
Can use subcontract welders qualified by AAA company WPS ??
Subcontractor welders qualified inside AAA company.
Please reply.
Shaunak.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40A8urMWfvbbo5iE9iR0BmfZDHSCYNfMtMtzZXO_xuWtyA%40mail.gmail.com.
Dear Sir,
The welder diameter qualification range is 73mm and above, as he welded 6inch pipe.
My question is can the above said welder can do welding on 2inch weldolet to run pipe connection, as the weldolet od if physically verified will be more then 73mm.
Regards
Vikas
Dear All,
One question
ASME JOB - ASME U STAMP certified company name ABC -
Can use subcontract welders qualified by AAA company WPS ??
Subcontractor welders qualified inside AAA company.
Please reply.