Dear all,

I want to weld 2inch weldolet to 24inch pipe, my doubt can i use welder qualified as per section 9 with diameter range 73mm and above to weld 2 inch weldolet whose OD is above 73mm.
Second doubt how much weld i need to deposit on weldolet to run pipe connection if code of construction is asme B31.3, i think it should be minimum thickness of branch or run pipe thickness and then make fillet. Or is it needed to deposit weld upto bevel end then a fillet.

Regards

Vikas

Patel Vivek

unread,
Oct 15, 2016, 11:32:09 AM10/15/16
to material...@googlegroups.com

Dear vikas,

You have to qualify welder in 2 inch to weld that weldolet on 24 inch pipe....

Regards,
Vivek


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BCgecnc-uScigVNxcd15GJQmb8ZhT-SWKO2eoFX%2BJhg7%2Bkpyw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

anthony chundal

unread,
Oct 16, 2016, 2:05:58 AM10/16/16
to material...@googlegroups.com

Dear all,

Thickness of both base materials also shall be considered as per Qw202.

Regards,
Anthony.


Vikas Waghmare

unread,
Oct 17, 2016, 1:27:43 AM10/17/16
to material...@googlegroups.com

Dear Friend,

2" Weldolet od will be more than 73mm and section 9 talks about OD.
My interpretation says we can weld , is there any code case or interpretation file number regarding same, if any of you arr aware please share.

Regards

Vikas


George Dilintas

unread,
Oct 18, 2016, 11:47:36 PM10/18/16
to Meghanadh K
If I understand correctly your input the welder was qualified with a pipe with OD=73 mm. In that case his is qualified for OD 25 mm and over.
Please note that base metal thickness is not an essential variable for welders qualification. Only the thickness of deposited metal.
Please check also the other essential variables before you proceed


For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Vikas Waghmare

unread,
Oct 19, 2016, 4:20:42 AM10/19/16
to material...@googlegroups.com

Dear Sir,

The welder diameter qualification range is 73mm and above, as he welded 6inch pipe.
My question is can the above said welder can do welding on 2inch weldolet to run pipe connection, as the weldolet od if physically verified will be more then 73mm.

Regards

Vikas


Shaunak Upadhyay

unread,
Oct 19, 2016, 4:21:04 AM10/19/16
to material...@googlegroups.com

Dear All,

One question
ASME JOB - ASME U STAMP certified company name ABC -

Can use subcontract welders qualified by AAA company WPS ??
Subcontractor welders qualified inside AAA company.

Please reply.
Shaunak.


dilintas

unread,
Oct 19, 2016, 11:46:08 AM10/19/16
to Meghanadh K
Give the exact ODOS of the qualification sample



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Vikas Waghmare <vikas.wa...@gmail.com>
Date: 19/10/2016 07:00 (GMT+01:00)
Subject: Re: [MW:25566] Welder qualification query

Dear Sir,

The welder diameter qualification range is 73mm and above, as he welded 6inch pipe.
My question is can the above said welder can do welding on 2inch weldolet to run pipe connection, as the weldolet od if physically verified will be more then 73mm.

Regards

Vikas

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BCgecmyn9NDBNkGa8M2fob0ou%3D9P37j2r975qsOGn8biUXJjw%40mail.gmail.com.

dilintas

unread,
Oct 19, 2016, 11:47:02 AM10/19/16
to Meghanadh K
No



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Shaunak Upadhyay <shanup...@gmail.com>
Date: 19/10/2016 07:48 (GMT+01:00)
Subject: Re: [MW:25566] Welder qualification query

Dear All,

One question
ASME JOB - ASME U STAMP certified company name ABC -

Can use subcontract welders qualified by AAA company WPS ??
Subcontractor welders qualified inside AAA company.

Please reply.
Shaunak.