Dear Experts,

   Our project (dosing tank) requires welding of SS316/316L plates of 5mm and 6mm Thickness, while welding of 6mm thickness with back weld, after welding on side-1 and back grinding from other end, we are observing porosity in the centre line with intermittent space during first and second phase. (attached LPT photo for reference)

   Kindly request, to advice your guidance for rectification.
Regards

Raju Kandula
WhatsApp Image 2019-05-31 at 3.42.13 PM.jpeg

Gopalakrishnan G

unread,
Jun 1, 2019, 12:58:47 PM6/1/19
to material...@googlegroups.com
Due improper baking of electrodes 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALwNT%2B_L0fTF7to9_9H97mQpGNZiY9yo7jbZEExcW4%2BexCFEwg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Babur Khan

unread,
Jun 1, 2019, 12:58:47 PM6/1/19
to material...@googlegroups.com
Dear Mr. Raju,
Please share also welding process, after reviewing attached image my opinion is porosity due to contamination or poor cleaning. (As per picture it’s showing on edges)

Muhammad Babur Khan
Sent from my iPhone
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALwNT%2B_L0fTF7to9_9H97mQpGNZiY9yo7jbZEExcW4%2BexCFEwg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
<WhatsApp Image 2019-05-31 at 3.42.13 PM.jpeg>

Bgav Sampath

unread,
Jun 2, 2019, 1:44:17 AM6/2/19
to material...@googlegroups.com

I think it may be lack of root fusion could you send me welding procedure for further details. And I can help you

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

george keribo

unread,
Jun 21, 2019, 2:43:32 AM6/21/19
to Materials & Welding
Dear Expert,
My opinion is that the porosity is caused due to improper cleaning before welding, It occurred on the same line. 

Vaishakh Kc

unread,
Jun 21, 2019, 4:23:19 AM6/21/19
to material...@googlegroups.com
Dear Mr Raju,
Mention the welding process. I think the welding were done in a contaminated place.
Thanks and Regards
Vaishakh kc

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.

Vinay Thattey

unread,
Jun 23, 2019, 10:57:27 AM6/23/19
to material...@googlegroups.com
DEAR RAJU:
This porosity is most likely due to contamination or moisture content. Bake the electrode . Environmental control is also necessary . Use only quality electrode. for

On Fri, 21 Jun 2019 at 13:53, Vaishakh Kc <vaish...@gmail.com> wrote:
Dear Mr Raju,
Mention the welding process. I think the welding were done in a contaminated place.
Thanks and Regards
Vaishakh kc
On 21-Jun-2019 12:13 PM, "george keribo" <bere...@gmail.com> wrote:
Dear Expert,
My opinion is that the porosity is caused due to improper cleaning before welding, It occurred on the same line. 

On Friday, May 31, 2019 at 2:01:01 PM UTC+1, Kandula Raju wrote:
Dear Experts,

   Our project (dosing tank) requires welding of SS316/316L plates of 5mm and 6mm Thickness, while welding of 6mm thickness with back weld, after welding on side-1 and back grinding from other end, we are observing porosity in the centre line with intermittent space during first and second phase. (attached LPT photo for reference)

   Kindly request, to advice your guidance for rectification.
Regards

Raju Kandula

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages