Eddy Current vs Hydrotest for LTCS pipes (A333 Gr.6)

93 views
Skip to first unread message

Eric.C

unread,
May 7, 2015, 1:39:04 AM5/7/15
to material...@googlegroups.com
Hi All,

Mill performed ET for 1.5" Sch160 Smls Pipe A333 Gr.6.
Is ET acceptable in lieu of hydrotest? if yes, is there any limitation criteria?
Thanks.

Regards,
Eric.C

Ritesh Rajput

unread,
May 7, 2015, 2:52:57 AM5/7/15
to material...@googlegroups.com
it is acceptable .

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/725e2e6d-7969-4d55-ab84-a02452545612%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

george....@gr.bureauveritas.com

unread,
May 7, 2015, 2:54:06 AM5/7/15
to material...@googlegroups.com

Yes if performed in accordance with the requirements of A-999

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for "Eric.C" ---07/05/2015 08:43:18---Hi All, Mill performed ET for 1.5" Sch160 Smls Pipe A333 Gr.6."Eric.C" ---07/05/2015 08:43:18---Hi All, Mill performed ET for 1.5" Sch160 Smls Pipe A333 Gr.6.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/725e2e6d-7969-4d55-ab84-a02452545612%40googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Alan Denney

unread,
May 7, 2015, 5:42:53 AM5/7/15
to material...@googlegroups.com

I have now looked at ASTM A 333 and see that eddy current testing is permitted as an alternative to hydrostatic testing under this standard. It goes to show – if all else fails read the specification!

 

From: Alan Denney [mailto:al...@denney1.freeserve.co.uk]
Sent: 07 May 2015 08:25
To: 'material...@googlegroups.com'
Subject: RE: 23220] Eddy Current vs Hydrotest for LTCS pipes (A333 Gr.6)

 

No. Eddy current test is a surface inspection technique – technically an alternative to MPI.

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Eric.C
Sent: 07 May 2015 02:25
To: material...@googlegroups.com
Subject: [MW:23220] Eddy Current vs Hydrotest for LTCS pipes (A333 Gr.6)

 

Hi All,

--

Reply all
Reply to author
Forward
0 new messages