Consumable Required to weld base Metal A516 Gr-70

83 views
Skip to first unread message

Muhammad Azeem

unread,
Jul 22, 2021, 6:28:05 AM7/22/21
to Materials & Welding
Gents,
I need your kind assistance to explain the consumable can be used for this material, As I received from one vendor WPS with following consumable from root till fill/cap. As I know the tensile strength of the base metal is 70000 KSI So  consumable should have more ??

Root - ER-70S-2 -GTAW
Fill - E7018 - SMAW
EH12K/F7P8- SAW

Regards,

M.Azeem Iqbal
 0590071467

Vishwas Keskar

unread,
Jul 22, 2021, 6:39:12 AM7/22/21
to material...@googlegroups.com
70 KSI is the  minimum UTS  of SA 516 GR 70.

So all consumables shall have 70 KSI minimum  UTS.

For said mentioned consumables in below your mail ,  70 KSI minimum  is achieved for consumables.
So no problem at all.
Get WPS PQR reviewed approved before start of production Welding.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2fad85f4-5b42-44cb-9eb8-357c9414dfc3n%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages