Dear All,

Does ASME B 31.1 dictates alternate NDT method in lieu of Pressure test if it cannot be performed? There are times during in service repair work for Boiler external piping where Pressure test cannot be performed due to unavailability of isolation. Please share your expertise.

Regards
Vino Varghese

george....@gr.bureauveritas.com

unread,
May 20, 2015, 7:17:29 AM5/20/15
to material...@googlegroups.com

The NDT in lieu of Pressure Test is a PED approach and not a Code approach

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for Vino Varghese ---20/05/2015 13:19:23---Dear All, Does ASME B 31.1 dictates alternate NDT method in liVino Varghese ---20/05/2015 13:19:23---Dear All, Does ASME B 31.1 dictates alternate NDT method in lieu of Pressure test if

Regards
Vino Varghese

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAM7oz7BYx41cTAFgXkZfzBPbX%3DVOo7mmXnE1Qc04FO%2BsDcX5LA%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

manish kulkarni

unread,
Jun 3, 2015, 2:38:19 AM6/3/15
to material...@googlegroups.com
You can try sensitive leak test

Sent from Yahoo Mail on Android


From:"Vino Varghese" <vinopv...@gmail.com>
Date:Wed, 20 May, 2015 at 14:19
Subject:[MW:23301] ASME B 31.1 / Pressure test cannot be performed

--
Reply all
Reply to author
Forward
0 new messages