I thought the question was “How” not “Why”
From: material...@googlegroups.com [mailto:material...@googlegroups.com]
On Behalf Of BANG NGUYEN
Sent: Wednesday, December 19, 2012 7:00 PM
To: material...@googlegroups.com
Subject: [MW:16265] Re: THIO Test.
hi Zair,
periodic test for the amount of residual thiosulphate & silver thiosulphate present on the process film shall be carried out.
the test is to be followed the manufacture recommendation.
commonly, Radiograph films shall be interpretable minimum period of 5 years.
On Wednesday, December 12, 2012 6:13:24 PM UTC+7, ZAIR wrote:
Dear All,
Please help me... How to carry out Thio Test for Radiography films???
Is this mentioned in ASME sec V??
Please help me.. Am in a fix
Zair
--
To post to this group, send email to
material...@googlegroups.com
To unsubscribe from this group, send email to
materials-weld...@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.