Welder qualified in API1104 Standard with destructive testing re destructive test require for station piping.(sec-ix)

176 views
Skip to first unread message

HARISH VARUDE

unread,
Jul 30, 2020, 9:26:49 PM7/30/20
to material...@googlegroups.com
Respected all experts,

I have one welder who qualified in API standard (for line pipe,gas field)with DT reports but now we want to do his new qualification for station piping as per Section ix Standard,for his qualification destructive test again require or not.
Or radiography base we can qualify to him.

From
Herish varude
Mob.No.:-7990746918

José Juan Jiménez Alejandro

unread,
Jul 30, 2020, 10:31:10 PM7/30/20
to material...@googlegroups.com
You can qualify your welder with guided bend tests or radiography, although there are some P numbers that require only guided bend.
Regards!.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGP-YKLrY6EtcSGS%2Bqi_fBfMDSemr7awiFkDuACDb4EUoCSNfQ%40mail.gmail.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SUMMIT MÉXICO - TPI

https://www.linkedin.com/in/summit-m%C3%A9xico-tpi-760047137/

Móvil +52 1 812 352 4606

Skype: jjjimeneza





SENTHILKUMAR SWAMINATHAN

unread,
Jul 30, 2020, 11:02:57 PM7/30/20
to material...@googlegroups.com
Required DT & RT. 
Regards, 
--

in...@pieper-qsi.nl

unread,
Jul 30, 2020, 11:03:03 PM7/30/20
to 'SENTHILKUMAR SWAMINATHAN' via Materials & Welding

Thank you for your e-mail, unfortunately I’m out of office till Monday August 10th . In the meantime I will have minimum access to my e-mail account. When you didn’t receive an response before this date I will answer your e-mail on Monday August 10th.

Best Regards,


Herman Pieper

Raja Varman

unread,
Jul 31, 2020, 5:56:58 AM7/31/20
to material...@googlegroups.com
As per ASME SEC. 9, a welder can be qualified by volumetric testing method(RT).



என்றும் அன்புடன்,
Thanks & Regards,
RAJAVARMAN
+971561895584

--

HARISH VARUDE

unread,
Jul 31, 2020, 5:56:58 AM7/31/20
to material...@googlegroups.com
Dear sir,
P no is same


From
Herish varude
Mob.No.:-7990746918

Customer Care

unread,
Jul 31, 2020, 11:30:58 PM7/31/20
to material...@googlegroups.com

HELLO SENTHILCUMAR,

 

Before proceeding with the requalification of the welder under ASME Section IX, it should be verified if this welder qualified under API 1104 covered the essential and non-essential variables requested by ASME Section IX. If there is equality of criteria in the welding variables and the DT & RT, just by performing an x-ray as a test, it is valid too.

 

Regards,

 

Ramon Briceno

Metallurgical Engineer / Oil & Gas

Linkedin: www.linkedin.com/in/ramon-briceño-976265b5

ramon.i...@gmail.com

 

Sent from Mail for Windows 10

Reply all
Reply to author
Forward
0 new messages