Electrode Qualification Test

130 views
Skip to first unread message

Pushpraj Anand

unread,
Dec 9, 2010, 5:17:28 AM12/9/10
to material...@googlegroups.com
Dear all,
 
We want Electrode Qualification Test on Filler wire for MIG ER70S-6 AWS SFA number-5.18
 
Kindly suggest me- what is root gap between & what is the backing plate thickness for 12mm thickness plate.
 


--
Regards,
Pushpraj Anand

joshi jaydeep

unread,
Dec 9, 2010, 5:56:23 AM12/9/10
to material...@googlegroups.com
You can not have thickmess of 13mm for Electrode qualification of ER70S-6.
 
Refer SFA 5.18 Fig 1 (Page no. 408 of 2007 ASME Sec II C) for details of requirements. It will also give the answers of your other doubts.
 
 
Jaydeep Joshi

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

John Du Plessis

unread,
Dec 9, 2010, 5:39:57 AM12/9/10
to material...@googlegroups.com

 

 

 

The test piece dimensions etc are all given in the SFA 5.18 speification. Read It.

John du Plessis

Technology Manager

 

Tel: +27 (11) 298 2100

Tel: +27 (11) 298 2103 (Direct)

Fax: +27 (11) 836 6014

Mobile:+27  82 883 4970

www.saiw.co.za

 

This email and any files transmitted with it are confidential and may be legally privileged. They are intended solely for the use of the individual or entity to whom they are addressed. Access to this e-mail by anyone else is unauthorised, and any disclosure, copying, distribution or other use of this e-mail is prohibited and may be unlawful. We will not under any circumstances have any responsibility or liability arising out of or in connection with any unauthorised use of this e-mail. If you have received this email in error please notify the sender before deleting it.

 


--