Base material  : ASTM A333 GR.6 to A350 LF2 CL 1 or
 P.No 1 & Group No.1 to P.No. 1 & Group No.2
  Pipe 8'' Sch 20 & WN Flange 8'' Sch 20, Impact Test : - 46 ⁰C

Code-ASME B31.3
 
GTAW- ER80S-Ni1 and A#10

SMAW-E7018-1 and A# 1

1) is it possible that we can have different WELD CHEMISTRY A #1 and A#10 in the same PQR please clarify?


Regards
mmm

Patel Vivek

unread,
Oct 29, 2016, 11:52:45 PM10/29/16
to material...@googlegroups.com

Possible... But keep dash(-) in A number in both WPS & PQR......custom undiluted weld metal....but they have to comply your other mechanical requirements....


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/95a556c3-0e66-4ecc-bce5-1683debfa601%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

dilintas

unread,
Oct 29, 2016, 11:52:53 PM10/29/16
to Meghanadh K

What is not prohibited by the Code is permitted. in that case you will have two different deposited thickness also 


Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: mmm <must...@gmail.com>
Date: 28/10/2016 18:21 (GMT+02:00)
To: Materials & Welding <material...@googlegroups.com>
Subject: [MW:25619] LTCS PQR

Dear Experts,

Base material  : ASTM A333 GR.6 to A350 LF2 CL 1 or
 P.No 1 & Group No.1 to P.No. 1 & Group No.2
  Pipe 8'' Sch 20 & WN Flange 8'' Sch 20, Impact Test : - 46 ⁰C

Code-ASME B31.3
 
GTAW- ER80S-Ni1 and A#10

SMAW-E7018-1 and A# 1

1) is it possible that we can have different WELD CHEMISTRY A #1 and A#10 in the same PQR please clarify?


Regards
mmm

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

George Dilintas

unread,
Oct 31, 2016, 6:20:40 AM10/31/16
to Meghanadh K
In case you use process with active gas of flux you have to perform a chemical analysis to determine the A no


For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all
Reply to author
Forward
0 new messages