Hello Welding Experts

Attached here with a drawing of Slip on flange welding with a Pipe. As per ASME B 31.1/ASME Sec VIII Dev 1 what is acceptable value of 'y' i.e. distance between raised face flange and weld on pipe.


Regards


Dhanush P R


slip on flange welding.jpg

Dinesh Somwanshi

unread,
Feb 13, 2016, 4:51:30 AM2/13/16
to materials-welding
Dear sir,

Generally will be 3-4 mm max. If we extent then could be chances that flange serration get damaged.

Regards

Dinesh

DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER
AUTHORIZED WELDING / NDT / PAINTING INSPECTION PERSONNEL,
AWS - CWI , CSWIP 3.1
BGAS  Gr 2 / 3
NDT II -UT , RT , MT , PT, VT
00919881344135

असो द्यावी दया तुमच्या लागतसे पाया.

Pray for others, sometime, You might never need to pray for yourself again.....

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9113b938-df01-4973-8582-f1eb9b8729b0%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

pradip kumar Sil

unread,
Feb 13, 2016, 6:21:10 AM2/13/16
to materials-welding

anand gupta

unread,
Feb 13, 2016, 6:21:15 AM2/13/16
to material...@googlegroups.com
One thickness of pipe min to be left fillet weld.

regards
a p gupta
saudi

Sent from Yahoo Mail on Android


From:"DHANUSH PR" <pr.dh...@gmail.com>
Date:Sat, 13 Feb, 2016 at 12:37 PM
Subject:[MW:24277] welding of Slip on flange to Pipe

dili...@gmail.com

unread,
Feb 13, 2016, 6:53:32 AM2/13/16
to DHANUSH PR
See app. 2 of Div 2

Sent from my BlackBerry 10 smartphone.
From: DHANUSH PR
Sent: Σάββατο, 13 Φεβρουαρίου 2016 - 11:37
To: Materials & Welding
Subject: [MW:24277] welding of Slip on flange to Pipe
Reply all
Reply to author
Forward
0 new messages