Dear Experts,
During my review of the WPS, I noted that a 4 mm GMAW wire has been specified. However, this wire size is not listed in the manufacturer’s technical datasheet available on their website. Although the vendor has submitted the wire MTC, there appears to be a discrepancy between the documented specifications and the datasheet.
Additionally, I am surprised to observe that welding has reportedly been carried out at a current of 900 amps using this wire. I would appreciate your clarification on the feasibility and justification of this parameter, as it seems unusually high for GMAW applications.
Kindly provide your technical inputs and supporting references for the above points.
Best regards,
Nambi
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJuyB2UHi13C3OS7mrKVWStL5NMR1%2Bv-dxSAU8--FSK83X8z-A%40mail.gmail.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CACjjzi1sy%2BufT%3D8wbDGxCkjF6ej5V33nmsNdagpGtHq1rj9okA%40mail.gmail.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJuyB2WkChhOT3WEh2LE0Q3%2Bt_oYdnLJpVdXG97-ZFhAzJOoHQ%40mail.gmail.com.