Galvanized steels are zinc coated carbon steels(typically). Zinc removal prior to welding is advisable, as Zinc creates lot of fumes, plus Zinc deposition is done under acidic solutions, which may cause dissolution of hydrogen. Attached is the article which explains how to handle such steels and successfully welding them. Additionally, you may download this AWS standard so as to find the necessary resources for welding Galvanized steels.
Thanks.
Pradip Goswami.P.Eng, IWE.
Independent & Consulting Welding & Metallurgical Specialist
Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/
Email:pgos...@rogers.com,pradip....@gmail.com
Cell/Whasapp:1-905-9793232
From: material...@googlegroups.com <material...@googlegroups.com> On Behalf Of HARISH VARUDE
Sent: April 14, 2021 8:09 PM
To: material...@googlegroups.com
Subject: [MW:32247] Required sample copy of welding procedure Specification for Galvanized pipe welding..
Respected experts,
If any have sample copy of approved welding procedure with PQR for Galvanized pipe welding. Please share me for reference..
From
Herish varude
Mob.No.:-7990746918
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGP-YKKH_q2-DUfdTQ9T6T%2BOXSjAveADRzdhM8ci4MSugA%2B6xw%40mail.gmail.com.