Dear Experts,
Kindly suggest suitable filler wire for following base metal combination.
Parent Metal 1 Parent metal 2
1) ASTM A 217 GR C 5 ASTM A 217 GR CA15
2) ASTM A 217 GR C 12 ASTM A 217 GR CA15
3) ASTM A 217 GR WC 6 ASTM A 217 GR CA15
4) ASTM A 217 GR WC 9 ASTM A 217 GR CA15
Thanks & Regards,
|
Brajendra S Patel | Engineer -Welding |
|
|
|
Mob:+917057406907 |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Help save the environment - do you really need to print this e-mail?
|
||
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/D288AF0A8981664D8CC97F6CFF20756B388557C2%40XCELLMBX01.xcellinfra.india.
For more options, visit https://groups.google.com/d/optout.