Pradip,

 

Refer to Table 9 on page 21, and to Subsection 8.4.3 and its associated Figures 12 to 14 on pages 32 to 35.

 

Regards,

D. Thompson

TeamQualspec

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of pradip kumar Sil
Sent: Friday, July 01, 2016 11:20 PM
To: materials-welding
Subject: Re: [MW:25049] Thermocouple Quantity

 

Dear Rogelio,

 

I already searched AWS D10.10 but i did not get any clear idea regarding how many thermocouple to be used during welding/ PWHT  in piping.

 

Regards,

 

 

 

On Fri, Jul 1, 2016 at 2:26 PM, 'Rogelio Alegre' via Materials & Welding <material...@googlegroups.com> wrote:

Hi Pradip 

My suggestion is AWS D.10.10/D10.10M: 1999(R2009) – Recommended. Practices for Local Heating of Welds in Piping and. Tubing.
Kind regards 
Sent from my iPhone


On 1/07/2016, at 4:56 pm, pradip kumar Sil <prad...@gmail.com> wrote:

Dear Everybody,

How many thermocouple to be  attached in the weldment during Pwht  / During Preheating , we are following as per  Project Specification.

 

My Question is anywhere in the code/ Standard  is it mentioned ? Pls refer

Thanks in advance

Regards

Pradip  

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8kLFfRTB_R82axYxBN8dEJPvfpJhY%3Ddm2seXUp7wd3B4Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/F76B7425-8933-48C4-8CA2-F931A1F55EA8%40yahoo.com.ar.
For more options, visit https://groups.google.com/d/optout.

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8ng4zd90kNsg%2BvPnaVLc2cWoOw7qPJnd9aaSuMdte_2xg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Reply all
Reply to author
Forward
0 new messages