REQUEST

36 views
Skip to first unread message

Eseosa Agho Otoghile

unread,
Jun 4, 2024, 11:04:20 AM6/4/24
to Materials & Welding
Hello Guys, 
Please what kind of filler wire is used for the welding of Aluminium Steel.


Thank you and Best Regards, 

Eseosa Otoghile 

sridhar cn

unread,
Jun 7, 2024, 7:23:35 AM6/7/24
to material...@googlegroups.com
Pl. clarify whether it is aluminium-coated mild steel, pure Aluminium or Aluminium alloys.
If it is al. alloy, it's grade. 
Sridhar.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b8c73c5a-3e2b-4eb8-92b8-8a492c0fb20an%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages