Furnace Tubes Ni 35 Cr 45 material welding

80 views
Skip to first unread message

Narasimha Murthy

unread,
Apr 5, 2017, 8:04:42 AM4/5/17
to material...@googlegroups.com
Dear All,
Kindly provide me the suitable electrodes for welding of Furnace  Ni 35 Cr 45.


Regards,

J.N.Murthy

sajeed zaheer

unread,
Apr 6, 2017, 12:48:37 AM4/6/17
to material...@googlegroups.com
ER NICR-3

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BFBpuCU%3Dzf21aDPqp_p2yY9atFwwwaDwvXNu0eNdsNcNZignw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Vanchinath S.A.

unread,
Apr 6, 2017, 1:26:38 AM4/6/17
to material...@googlegroups.com
Use Thermanit 35/45 Nb filler wire for Gtaw process.

--

Mumtaz Ahmed

unread,
Apr 6, 2017, 1:43:26 AM4/6/17
to material...@googlegroups.com
you can use filler wire UTP A3545 NB for furnace tube material.


Regards
Mumtaz Ahmad
QA/QC Lead
Descon Engineering 
Borouge-UAE


To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B6Tn1L1mxcQTUi96VsjZhxirUfrccNU4dfgZj5Vid7SyLKYig%40mail.gmail.com.

Prakash Hegde

unread,
Apr 7, 2017, 11:47:23 AM4/7/17
to material...@googlegroups.com
Hi ! Friend
We have used earlier ENiCrF2 and ERNiCr3 for furnace tube welding
Regards
Hegde