API 650 - telltale hole in RF pad

175 views
Skip to first unread message

M S

unread,
Apr 29, 2012, 5:25:06 AM4/29/12
to material...@googlegroups.com
Dear Experts,


As per API 650, telltale hole shall be located substatially on the horizontal centerline. Could you please explain the reason. What will be the effect if the tellhole located at other locations?

Regards.

Srinivasulu Kalasapati

unread,
May 2, 2012, 1:36:31 AM5/2/12
to material...@googlegroups.com
Hi,
 
This is really intresting Question, for pipe when we are adding R-Pad the weep hole shall be on the opposite side of crotch.
 
Regards,
Srinivas

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Ohm Guru Namasivaya
Reply all
Reply to author
Forward
0 new messages