Submerged Arc Welding Process Wire/Flux Classification

95 views
Skip to first unread message

Prashant

unread,
Apr 4, 2024, 5:51:45 AM4/4/24
to Materials & Welding
For SAW welding wire/flux classification as an sample for discussion

As per A 5.17 it is represented as F7P8-EH12K, this classification is given by the product manufacturer on the flux bag and is inline with the ASME Sec II Part C SFA 5.17
Where P is pwht and 8 is Minus 80 Deg F Impact test

I have a Procedure qualification which is Impact tested at Minus 50 Deg F, Qualified as per ASME Sec IX
as per QW 404.9
is it correct I write on my Procedure qualification record
F7P5-EH12K

Please advise above is correct,  if not I would like to understand more on this what should be written and clarification to increase knowledge

Kurniatullah Sirajudin

unread,
Apr 6, 2024, 6:15:45 AM4/6/24
to material...@googlegroups.com
Dear prashant

That is corect

When you will prepare PQR with impact test and SAW process for carbon steel, you should be check temperature and compare with table 7 of ASME sect. IIC part SFA A5.17

Hope this can answer your question

Salam
Kurniatullah,IWE


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f81d62f2-1e20-456f-baee-0159e2ef3222n%40googlegroups.com.
Screenshot_20240404_194133_OneDrive.jpg
Screenshot_20240404_194323_OneDrive.jpg

Paidi

unread,
Apr 9, 2024, 9:29:44 AM4/9/24
to material...@googlegroups.com
Hello..

Below mail I Understand that Welding done with F7P8-EH12K and Impact test done @-50F and write PQR as F7P5-EH12K.

 

With reference to QW254 and 404.12 when impact testing applicable, Classification changes calls for requalification.

(Welded with higher grade (P8) filler wire combination. Writing lower grade (P5), hence production can be done with P5.

it is uncertain if welded with lower grade (P5) same combination of base metal, Impact test may not be compiling Impact value requirement )

 

 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f81d62f2-1e20-456f-baee-0159e2ef3222n%40googlegroups.com.


--
Thanks  & Best Regards,

Suresh Paidi


 
Reply all
Reply to author
Forward
0 new messages