High Carbon Steel is characterized by as having what type of weldability?

1.Very Good Weldability

2.Not Weldable

3.Good weldability with SMAW process

4.Good Weldablity

5.Poor


Can the IWE's in the group pls explain why the answer to this question is option 3? 

Ramin Kondori

unread,
Sep 23, 2020, 12:59:25 AM9/23/20
to material...@googlegroups.com
Dear Zacharias,

Carbon (in steel) always causes weldability issues.
It depends on the C-content and other elements (material's manufacturing process and heat treatment shall be taken into consideration). But in general, it makes it more difficult to weld.

You can easily find tons of useful information on this subject by googling "weldability of High Carbon Steels". Below, you can see examples of google's first page of search results for this: 

High carbon steels contain 0.60-1.0% carbon and 0.30-0.90% manganese. They are are very hard and strong, but also have poor weldability and are difficult to weld without cracking. Once heat treated, these are extremely hard and brittle.

The high carbon steels are difficult to weld because of the hardening effect of heat at the welded joint. Because of the high carbon content and the heat treatment usually given to these steels, their basic properties are impaired by arc welding. 
 
High carbon steel is even more prone to weld cracking than the other two groups of carbon steelWelding high carbon steel will most likely require very thorough preheating and post-heating processes to avoid this. It could also require special welding filler metals.  
 
Regards
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c75217b8-a8e8-4ddc-93f6-aafbdb137defn%40googlegroups.com.

Kannayeram Gnanapandithan

unread,
Sep 23, 2020, 2:09:53 AM9/23/20
to materials-welding
Because of variety of consumable is available for SMAW process, But welding is not easy like others, weldability is very poor. 

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


George Dilintas

unread,
Sep 23, 2020, 9:11:11 AM9/23/20
to material...@googlegroups.com
You  could weld them using the same method for welding cast iron.
I have done it and it works

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c75217b8-a8e8-4ddc-93f6-aafbdb137defn%40googlegroups.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all
Reply to author
Forward
0 new messages