Dear Experts,

I need ASME interpretation IX-86-43 for following query.

QW-202.4, Dissimilar Base Metal Thicknesses

Date Issued:     December 22, 2004

File No:            04-599

 

Background:  A procedure qualification test coupon using the same P-Number material and consisting of two plates of different thicknesses are welded together, where the thicker of the two plates (T2 = 1-1/2” thick) has been tapered on a 4:1 taper down to the thinner plate thickness (T1 = 1” thick).

 

Question (1):  Does this test coupon qualify the WPS for a base metal thickness range of 3/16” to 8”?

 

Reply (1):  See Interpretation IX-86-43, Question (2).



Thanks & Regards


Hiren Sevak


Rajagopal Kannan

unread,
Dec 2, 2012, 11:43:52 PM12/2/12
to material...@googlegroups.com
Dear Sir,
No. If the Weld is made without taper, This is qualified for the thickness range you mentioned. Now the thickness at weld joint is considered as 25 mm only. Hence the thickness range as per ASME sec. IX is 5 to 50mm.
Thanks and Best Regards,
K.Rajagopal


Hiren Sevak


--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

Reply all
Reply to author
Forward
0 new messages