EmaD FaRaHanI

unread,
Apr 15, 2021, 9:57:18 AM4/15/21
to material...@googlegroups.com
Dear all,
Tube A210 welding with GTAW or SMAW with thickness 5.5mm, obviously no access to the inside of the pipe. 
What is your suggestion? square butt or single v?

Thanks,

Prem Nautiyal

unread,
Apr 15, 2021, 11:18:58 PM4/15/21
to material...@googlegroups.com
GTAW
Single V..

Regards

Prem Nautiyal 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABtwbJFa2e_1dMQ3hiriryK7YYe5iuZQgP3S6UxVhugKEfL16w%40mail.gmail.com.

Alcindo Jardim

unread,
Apr 15, 2021, 11:18:58 PM4/15/21
to material...@googlegroups.com
for pipe always simgle V
Alcindo O. J. Jr.
21 96676-1511



--

Vishwas Keskar Welding Manager WELDING

unread,
Apr 18, 2021, 1:50:45 AM4/18/21
to Materials & Welding
Single Vee
Full GTAW process  