I have scenario in site, we have to qualify welders for cs to ss,but we dont have ss material available ,can we do with cs alone using f43 filler wire. wps- p5a to p8- f.no-43
Wqt - p5a to p5a- f.no-43

Thanks&regards

Aslam 


venkateswara reddy Desireddy

unread,
Feb 3, 2026, 3:00:06 AMFeb 3
to material...@googlegroups.com
We can use P5a. 




From: material...@googlegroups.com <material...@googlegroups.com> on behalf of Aslam Khan <akch...@gmail.com>
Sent: Tuesday, February 3, 2026 10:50:27 am
To: material...@googlegroups.com <material...@googlegroups.com>
Subject: [MW:35983] P5A to P8
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAA7Erp%3DnRb20byLE0w2M14GDcFF3G1wkuy-5FzsTxyCpp7Q0Tw%40mail.gmail.com.

Manoj Mumbai

unread,
Feb 3, 2026, 6:47:08 AMFeb 3
to material...@googlegroups.com
As per code you can use. 
Convince your customer also before starting WQT.

Thanks & Regards
Manoj

sridhar cn

unread,
Feb 3, 2026, 6:47:08 AMFeb 3
to material...@googlegroups.com

As per ASME Section IX, welder qualification for a dissimilar weld (P5A → P8) performed using F-No. 43 filler cannot be done on 

P5A → P5A materials alone. The test coupon must include at least one P8 base metal to represent the metallurgical condition of 

the production weld. Therefore WQT must be performed on a CS + SS test coupon. CS + CS coupon with F43 is not acceptable under

ASME IX.

Sridhar.


Anandhapadmanabha pillaim

unread,
Feb 3, 2026, 7:15:39 AMFeb 3
to material...@googlegroups.com
As per ASME SEC IX QW-423 Which allows alternative materials for welder qualification and the welder will be qualified within the ranges of the essential variable, you can proceed with WQT on a P1 to P1 material with F43.


Aslam Khan

unread,
Feb 3, 2026, 7:15:39 AMFeb 3
to material...@googlegroups.com
What about qw-423, it mention we can use alternative material for wqt,pls clear the doubt

Thanks&regards

Aslam khan
Mob:+965 66744128




Anandhapadmanabha pillaim

unread,
Feb 3, 2026, 8:52:19 AMFeb 3
to material...@googlegroups.com

Qw-423 Allows alternative material for WQT.

You can alter the base material mentioned in the WPS , alternative base material shall be chosen as per the table mentioned in QW-423.

Kannayeram Gnanapandithan

unread,
Feb 5, 2026, 1:10:18 AMFeb 5
to material...@googlegroups.com
Good Engineering Practice is to be followed eventhough Code allows because metal flow is very important. Mock up test is to be done before engaging in the work.
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085, 
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


Reply all
Reply to author
Forward
0 new messages