RT JOINT FILM SIDE SOURCE SIDE IQI

54 views
Skip to first unread message

Mohd Siraj

unread,
Apr 18, 2016, 1:26:08 AM4/18/16
to Materials & Welding
DEAR ALL,

IS THERE ANY WAY TO.FIND THAT RT IS TAKNE WITH IQI FILM OR SOURCE SIDE BY FILM ITSELF.
I KNOW LETTER F.
IS THERE ANY WAY TO COUNTER CHECK?

MAT CS AND SS THK 3.91 -7.11 PIPES.

tha...@alpha-ecc.com

unread,
May 7, 2016, 5:06:28 AM5/7/16
to Materials & Welding
Because you not mention OD pipe, so I dont know which technique using.
For SWSI technique: No way to counter check.
For DWSI/DWDI, you can compare distance from 02 wire IQI at RT film and distance actual. If it's same. IQI at film side.