hido we need preheat of electrode when using inconel-625
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e9e2daff-7d56-4611-aa40-97edced03eef%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Yes...
These electrodes are basic coated.
And hygroscopic in nature...