ASME SA 333 Gr. 6 Chemical composition

544 views
Skip to first unread message

Azam Mohd

unread,
Mar 13, 2013, 8:35:56 AM3/13/13
to material...@googlegroups.com

Dear Experts,

The below material chemical composition for ASME SA 333 Gr. 6 as per MTC

 

 

But as per ASME SA 333 Gr.6, Allowable chemical element C, Mn, P, S, Si only. Please refer ASME Section II Part A Edition 2010 clause 5.2.

 

Need your comment weather this chemical composition can be accepted. Please provide the technical clarification or code reference.

 

Thanks & Regards,

Mohd. Azam


image002.png

Azam Mohd

unread,
Mar 27, 2013, 5:53:31 AM3/27/13
to material...@googlegroups.com

Dear All Experts,

Please provide your feedback for below query with some technical justification or code reference.

 

Thanks & Regards,

Mohd. Azam


On Tue, Mar 19, 2013 at 5:09 PM, Azam Mohd <azam...@gmail.com> wrote:

Dear Experts,

ASME Section II Part A Edition 2010

ASME SA 333/SA 333M

 

The Pipe material is ASME SA 333 Gr.6, as per clause 5.2 and Table-1 the allowable chemical element is C, Mn, P, S, Si only

As per material MTC chemical element is C (0.17%), Mn (093%), P (0.010), S (0.0010), Si (0.24), Cu(0.050%), Cr (0.12%), Ni (0.060%), Mo(0.020%), V(less than 0.004%).

 

Our query is weather above chemical element (MTC) can be accepted for ASME SA333 Gr.6.

 

Looking forward to see the comment from Mr.Pradip Goswami on above matter.

 

Thanks & Regards,

Mohd. Azam

Doha-Qatar

image002.png

sajeed zaheer

unread,
Mar 30, 2013, 3:08:44 AM3/30/13
to material...@googlegroups.com
Dear Azam,
as per sec 8 div 1 partA  pg.550 para 5 chemical composition,

THE ADDITION OF ELEMENT REQUIRED FOR THE DEOXIDATION OF THE STEEL IS PERMITTED. AND YOU CAN ACCEPT THE ABOVE MENTION MTC AS PER THIS PARAGRAPH. 


--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

image002.png

george....@gr.bureauveritas.com

unread,
Mar 30, 2013, 9:05:07 AM3/30/13
to materials-welding

Sorry
But which of the additional elements is used for deoxidazation?
Usually for deoxidazation Al or Ca is used
Best regards
Dr Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
HBS Regional Technical Manager


This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com
image002.png
Reply all
Reply to author
Forward
0 new messages