Procedure Qualification Record

57 views
Skip to first unread message

Anumiah Veera Jegan

unread,
Jan 4, 2021, 5:10:30 AM1/4/21
to Materials & Welding
Dear experts,

The base materials to be used in the project are based on BS EN 10025-2 : 2004 Grade S275JR.Can I qualify my procedure based on API 1104?. If so,can you please advice me on the grade of the base materials which can be used for the procedure qualification?.

Thanks.

The information contained in this e-mail may be privileged and confidential. If the reader is not the intended recipient, or agent of the intended recipient, any unauthorised use, disclosure, copying, distribution or dissemination is strictly prohibited. If you have received this communication in error, please notify the sender immediately and delete it from your system.

Vishwas Keskar

unread,
Jan 4, 2021, 5:21:43 AM1/4/21
to material...@googlegroups.com
S275 JR is basically  material used for Structural  application.
I hope  , your application also is for structures .
For welding qualification ,  you can use AWS D1.1  OR  EN 15614

AWS D1.1 is well accepted  by Clients .
You have to qualify procedures/ Welders.



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6274779e-16d4-447f-9636-cbb818c9105cn%40googlegroups.com.

Anumiah Veera Jegan

unread,
Jan 4, 2021, 5:35:19 AM1/4/21
to Materials & Welding
Dear Vishwas,
As per the client , the procedure is to be qualified based on API 1104.Can you please advice me on the base material selection for Procedure/Welder qualifications?

Ganesh Muthurajan

unread,
Jan 4, 2021, 10:23:45 PM1/4/21
to material...@googlegroups.com
It's structural steel ASTM - A36
You go for E 7018 SMAW 

Pre qualilified WPS are available with AWS D 1.1

please look on it.

Ganesh,
QCI Welding.

--