Dear Experts,
I want to approve an FQP for Pipe erection, and in that FQP I want to mention the tolerance limit for the straightness of the pipeline.
I had also referred to relevant specifications and different codes including ASME B31.3 process piping but acceptance criteria is not mentioned anywhere.
Please suggest on which basis I can mention the tolerance limit for straightness of the pipeline in FQP.
--