Hello everyone, hope you are doing well

Does anyone have welding visual images of different defects and explaining the post weld inspection process?, any document related to the above will be very much helpful.

Thanks and Regards
Shahil Saini 
PGET-Welding

sridh...@yahoo.com

unread,
Feb 6, 2022, 7:01:45 AM2/6/22
to material...@googlegroups.com
Dear Mr. Shahil Saini,

Enclosing the post weld defects - visual images, its definition and main causes for your study.
and hope this may help you.

C Sridhar.
---------------------------------------------------------------------------------------------------------------


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_-zqhRmi-%2BJOjwHtj%2BYfWzxzLXM5ysouw0s1JLW15KFxw%40mail.gmail.com.
WELD DEFECTS - CS.pdf

chandrakant mohikar

unread,
Feb 6, 2022, 10:20:39 PM2/6/22
to material...@googlegroups.com
Please find attachment for welding defects images