Hi Sachin,
I hope API RECOMMENDED PRACTICE 945, Avoiding Environmental Cracking in Amine Units is refereed in the drawings. This is an essential document for amine service .As per this document use of austenitic S.S (304L/316L) clad steel is often done for amine plant equipments, for specific set of design conditions. That’s well taken care of in the details provided below.
As regarding fabrication, PWHT requirement is governed by the thickness of the backing material Carbon Steel, for regular amine service. From that aspect had this been a normal Amine vessel with 316L clad, exemption from PWHT would have been possible for 8 mm of C.S wall thickness.
Sec-VIII, UW-2 refers to mandatory PWHT for C.S/LAS vessels in “Lethal Service” . The same concept is applicable for clad vessels also, involving lethal service. Please see the latest ASME Code interpretations as below. Note there are two answers. My interpretation is to go with tracking No 9980 (since it’s latest and more detailed)
Hope this would help.
Thanks.
Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist &
Consultant.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions w.r.t.
applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups
"Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email
to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160401172500.21291.qmail%40f5mail-224-128.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.
Dear Sachin,
Check your project specification & process data sheet requirements.
Technically you can perform perform PWHT.
Regards,
Vijay Patre
--
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPi2c28zg9DbN%2Bv1Xfmp38ox5i_9-U1Mm%2BZgpqgnFe0gj1pGDg%40mail.gmail.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAAHsE2gzSxr1MjMVWF%2B9WUPABAAAAAA%3D%3D%40quickclic.net.
For more options, visit https://groups.google.com/d/optout.
Ing. Jose Juan Jimenez Alejandro
Cel. 8116171750
Skype: jjjimeneza
| From: Kannayeram Gnanapandithan Sent: Κυριακή, 3 Απριλίου 2016 - 08:44 To: materials-welding Reply To: material...@googlegroups.com Subject: Re: [MW:24622] Lethal service requirement |
| From: pgoswami Sent: Κυριακή, 3 Απριλίου 2016 - 07:11 Reply To: material...@googlegroups.com Cc: sachin...@rediffmail.com; 'Mainak Mukherjee' Subject: [MW:24618] RE: 24612] Lethal service requirement |